Ref the gas lenses, I looked for them in Australia awhile ago but no welding supply places seem to have them. Do you have a link to a supplier who takes PayPal and ships internationally?
Thanks in advance
Moderator: Site Moderator
hey thanks... no specialty just a regular Alberta certified journeyman welder with an interprovincial red seal, i think once you do out of position work ie tig roots on pipe and get decent at that you can do very well in the easier positions flat for example or positioning pipe for max comfort. i am an impeccably good fitter though and i do contract welding of all sorts.johnhopper1957 wrote:I have got to say they are the nicest welds I have seenI am guessing you do specialised stuff on the TIG?
Ref the gas lenses, I looked for them in Australia awhile ago but no welding supply places seem to have them. Do you have a link to a supplier who takes PayPal and ships internationally?
Thanks in advance
Not surprised it dulled your stainless. Muriatic acid (hydrochloric acid) is no good for pickling (passivation). Has the opposite effect.mash rookie wrote:I tried Muratic acid first. An overnight soak at 50% solution dulled the stainless and removed some but not all of the black discoloration.