Passivation gel/paste
Moderator: Site Moderator
-
Novice
- Swill Maker
- Posts: 189
- Joined: Fri Aug 22, 2025 2:55 pm
Passivation gel/paste
I'm mixing up some corn starch and 15 % citric acid to go over some fitting I added to some 304 kegs and a 20l milk can. In making the paste I don't believe I need to heat it up, but my lack of memory makes me question my idea. So what does the herd think?
- Corn Cracker
- Posts: 1402
- Joined: Sun Jun 13, 2021 7:25 am
- Location: s.e. Texas
Re: Passivation gel/paste
I think you need to heat the corn starch and water to thicken/gel it, add citric and apply it to the spot
I think I'll go home and fire up my still, it might not make me feel better but, I bet it will
-
MooseMan
- Master of Distillation
- Posts: 3312
- Joined: Fri May 28, 2021 4:54 am
- Location: Wales UK
Re: Passivation gel/paste
I've always just mixed citric granules into a gritty paste with water and used it like that, no heating. Just wipe dry after a few hours.
Make Booze, not War!
-
Novice
- Swill Maker
- Posts: 189
- Joined: Fri Aug 22, 2025 2:55 pm
Re: Passivation gel/paste
A lot of articles say you need to soak ss in hot citric acid to get passivation. I have some kegs I used the cornstarch method on and have no rust. But I don't know it I really needed to do that after silver soldering a fitting. I have some tigged fitting I need to work on now.Corn Cracker wrote: ↑Mon Nov 02, 2026 4:27 pm I think you need to heat the corn starch and water to thicken/gel it, add citric and apply it to the spot
- Corn Cracker
- Posts: 1402
- Joined: Sun Jun 13, 2021 7:25 am
- Location: s.e. Texas
Re: Passivation gel/paste
With solder I think your fine, it's high heat brazing and welding that discolors it.
I think I'll go home and fire up my still, it might not make me feel better but, I bet it will
- BigSwede
- Distiller
- Posts: 1012
- Joined: Thu Feb 06, 2014 10:36 am
Re: Passivation gel/paste
You can passivate at lower temperatures, it simply requires a longer exposure. If using some sort of paste, maybe apply the paste and then cover with some plastic wrap to keep it moist.
When I passivated my structured packing material, the recommendation was 10 minutes at just below a water boil, or 30 minutes at room temp. Seemed to work fine.
The other thing to consider is a thorough degreasing of the spot or material to be passivated.
When I passivated my structured packing material, the recommendation was 10 minutes at just below a water boil, or 30 minutes at room temp. Seemed to work fine.
The other thing to consider is a thorough degreasing of the spot or material to be passivated.