CCVM packing?

Vapor, Liquid or Cooling Management. Flutes, plates, etc.

Moderator: Site Moderator

Post Reply
Sailman
Rumrunner
Posts: 556
Joined: Wed Aug 21, 2019 7:02 am

CCVM packing?

Post by Sailman »

I'm rolling up some copper mesh to finish my CCVM. Since this already came in relatively clean do I need to run this through the vinegar run and the sacrificial run or is just a sacrificial run OK?
You do not have the required permissions to view the files attached to this post.
User avatar
Saltbush Bill
Global moderator
Posts: 11638
Joined: Thu Mar 17, 2011 2:13 am
Location: Northern NSW Australia

Re: CCVM packing?

Post by Saltbush Bill »

Ive heard it said that it can have oil from the manufacturing process on it, some people boil it I think, or you could put it in the still while doing the cleaning run.
MooseMan
Master of Distillation
Posts: 3294
Joined: Fri May 28, 2021 4:54 am
Location: Wales UK

Re: CCVM packing?

Post by MooseMan »

My fine copper mesh came on big rolls from an industrial supplier and 100% had some kind of oil on it, probably just to keep it from oxidising on the shelf?

I packed the column, ran boiling water, then vinegar, then sac run.
The water came out filthy, oily and cloudy green, the vinegar much less so and clean by the end, and the sac run looked and smelled clean so I was happy that I'd cleaned it to my best ability.
Make Booze, not War!
User avatar
Saltbush Bill
Global moderator
Posts: 11638
Joined: Thu Mar 17, 2011 2:13 am
Location: Northern NSW Australia

Re: CCVM packing?

Post by Saltbush Bill »

I washed mine in foreshots then put it in the still and did a cleaning run......that was a long time back now......since then it's had a couple of cleans in hot dunder.
Post Reply